ElgiloyUNSR30003W.Nr2.4711ApplicationsSprings,seals,semiconductorcomponents,orthodontics,medicaldevices,surgicalimplants,satellitecommunicationsequipment,andweaponssystems.DescriptionElgiloy isanon-magneticCobalt-Chromium-Nickel-Molybdenumalloyh*ingauniquecombinationofveryhighstrengthwhilemaintainingexcellentformability,excellentcorrosionresistance,andhighfatiguestrength.Additionalstrengthincreasesofupto25%canbeachievedthroughagingcoldreducedmaterial.Elgiloy ishighlyresistanttosulfidestresscorrosioncracking,andasaresultisthealloyofchoiceinthemostdemandingsourwellenvironments.Inseawater,Elgiloy isvirtuallyimmunetocreviceandstresscorrosionandpittingevenatthehigheststrengthlevels.Elgiloy performsacrossawiderangeoftemperatures:fromcryogenicupto850°F (454°C).IndustriesSuppliedOil&GasExtraction,Medical,Dental,Aerospace,Defense,SpaceExplorationandWatchmaking.NominalCo*itionC:0.15maxMn:1.5-2.5Si:1.20maxP:0.015maxS:0.015maxCr:19.0-21.0Ni:14.0-16.0Co:39.0-41.0Mo:6.0-8.0Be:0.10maxFe:BalancePhysicalPropertiesDensity: 0.30lb/in3,(8.30g/cm3)ModulusofElasticity(E): At70°F(20°C):27.0x 103 ksi(190GPa)ModulusofRigidity(G): At70°F(20°C):11.0x103 ksi(76GPa)CoefficientofExpansion:8.4in/in.-°F(70°Fto600°F)15.2m/m-°C(20°Cto300°C)ElectricalResistivity: 39.21Ω.in,(99.6Ω.cm)ThermalConductivity: 86.5Btu-in/ft2hr-°F,(12.5W/m-K)ApplicableSpecificationsStripandFoil: AMS5876,ASTMF1058,NACEMR0175&MR0103,ISO5832-7TypicalMechanicalProperties–SpringApplicationsAnnealedHeatTreatment: PerAMS5876TensileStrength: 100ksimin(690MPa)SuggestedOperatingConditions: -300°F to850°F (-184°C to454°C)SpringTemperHeatTreatment: NoHeatTreatmentTensileStrength: Upto310ksi(2100MPa)SuggestedOperatingConditions: -300°F to850°F (-184°C to454°C)SpringTemper+AgedHeatTreatment: Aftercoldrolling.Age:PerAMS5876,NaceMR0175TensileStrength: Upto380ksi(2600MPa)SuggestedOperatingConditions: -300°Fto850°F(-184°Cto454°C)标签:Elgi埃尔吉洛钴铬镍合 Elgiloy埃尔吉洛伊非磁性合金钴铬镍合金 上海市非磁性合金 上海市非磁性合金厂家上海市上海市[Elgiloy
埃尔吉洛伊非磁性合金
钴铬镍合金]
上海市非磁性合金厂家Elgiloy(40Co-20Cr-16Fe-15Ni-7Mo)埃尔吉洛伊非磁性合金钴铬镍合金化学成分物理性能